In this economically flourished area, there are many people who know the airflow pulverizer, and Turbo Mill of Plaster technology is in a leading position in the same industry.
Turbo Mill of Plaster will rise in the working fluid. When the temperature of the working fluid is too high, the flow rate of the gas will increase. Taking air as an example, the critical speed at room temperature is 320 m / sec, and when the temperature rises to 480 ° C, the critical speed can be increased to 500 m / sec, that is, the kinetic energy increases by 150%. Therefore, increasing the temperature of the working fluid is conducive to improving pulverization. The pressure of the working fluid is the main parameters of the jet speed, but also the main parameters affecting the fineness of the break. Typically, the higher the pressure of the working fluid, the faster the speed, the greater the kinetic energy.
When titanium powder is pulverized by superheated steam, the vapor pressure is usually from 0.8 to 1.7 MPa, and generally pulverized calcined material is high, and the material after the pulverized surface is low.
Technical parameters:
Finished granularity: D50: 0.8-5μm
Production capacity: 4.5 +/- 10% / T